As a professional high quality Gearbox Anti Erosion Wrapped Bronze Bearing manufacturers, you can rest assured to buy Gearbox Anti Erosion Wrapped Bronze Bearing and we will offer you the best after-sale service and timely delivery.
As a professional high quality Gearbox Anti Erosion Wrapped Bronze Bearing manufacturers, you can rest assured to buy Gearbox Anti Erosion Wrapped Bronze Bearing and we will offer you the best after-sale service and timely delivery.
Material: |
Tin-Bronze CuSn8Pfills With Special Solid Lubricant In The Sockets |
Types: |
Wrapped Bushes, Thrust Washer |
Application: |
In Conditions Of Heavier Load But Mediate Running Velocity, Such As On Engineering Machines, Gearbox, And Clutch On The Automotive Vehicles, Etc. |
Heat Conducting Coefficient: |
58 W/(m*k) |
Max. PV Value: |
2.8N/mm²·m/s |
Max. Load Pressure: |
100N/mm² |
High Light: |
bronze thrust washer, bronze bearings |
Gearbox Anti Erosion Wrapped Bronze Bearing With Special Solid Lubricant
It is made of Tin-bronze CuSn8P that is of high density. Its surface is punched with oil sockets by certain angle and density. There fills with special solid lubricant in the sockets, which endows the products with fairly small friction coefficient. Therefore, it can maintain a good lubrication capability when oil is temporarily run out. In addition, It has good anti-fatigue and load, anti-erosion and abrasion capacity. The products are widely applied in conditions of heavier load but mediate running velocity, such as on engineering machines, gearbox, and clutch on the automotive vehicles, etc.
Product NO. | Chemical Compositions | ||
TOB 093 | Cu | Sn | P |
91.3 | 8.3 | 0.2 |
Performance Index | Data | Performance Index | Data | |
Max. Load Pressure | 100N/mm² | Mating Axis | Hardness | ≥50 HRC |
Max. Linear Velocity | 2 m/s | Roughness | Ra=0.4~1.0 | |
Max. PV value | 2.8N/mm²·m/s | Max. Working Temperature | 150℃ | |
Tensile Strength | 460N/mm² | Friction Coefficient | μ 0.05~0.20 | |
Yield Strength | 260N/mm² | Heat Conducting Coefficient | 58 W/(m*k) | |
Hardness | HB 90~150 | Heat Expansion Coefficient | 18.5 10^-6k^- |