As the professional manufacturers, Top Bearings would like to provide you High Speed Bimetal Bearing Thrust Washer. And we will offer you the best after-sale service and timely delivery.
As the professional manufacturers, Top Bearings would like to provide you High Speed Bimetal Bearing Thrust Washer. And we will offer you the best after-sale service and timely delivery.
Material: |
Low Carbon Steel Wth Tin-Lead-Bronze Alloy (CuSn4Pb24) |
Types: |
Bimetal Thrust Washer |
Application: |
Main Shaft And Con Rod Shaft Of Internal Combustion Engine With Heavy Duty Capacity And High Speed |
Alloy Hardness: |
HB 45-70 |
Max. Load: |
130N/mm² |
Max. Working Temperature: |
Grease Lubrication Is 150℃, Oil Lubrication Is 250℃ |
High Light: |
bearing thrust washer , steel flange bearing |
CuSn4Pb24 Bimetal Thrust Washer is backed with high quality low carbon steel with Tin-Lead-Bronze alloy (CuSn4Pb24) sintered on its surface.
CuSn4Pb24 Bimetal Thrust Washer is with very high fatigue-resistance, load capacity, impact ability, and corrosion-resistance.CuSn4Pb24 Bimetal Thrust Washer is widely used in main shaft and con rod shaft of internal combustion engine with heavy duty capacity and high speed.
To effectively decrease abrasion, CuSn4Pb24 Bimetal Thrust Washer' alloy surface can be machined with oil grooves for easier oil storage. When necessary, an erosion protection coating can be plated on the steel back. In common application.
CuSn4Pb24 Bimetal Thrust Washer is widely used in main shaft and con rod shaft of internal combustion engine with heavy duty capacity and high speed.
Performance Index |
Data |
Performance Index |
Data |
||
Max. Load |
130N/mm² |
Mating Axis |
Hardness |
≥48 HRC |
|
Linear Velocity |
Grease Lubrication |
2.5 m/s |
Roughness |
Ra=0.16~0.63 |
|
Oil Lubrication |
10 m/s |
Max. Working Temperature |
Grease Lubrication |
150℃ |
|
Max. PV value |
Grease Lubrication |
2.8N/mm²·m/s |
Oil Lubrication |
250℃ |
|
Oil Lubrication |
10N/mm²·m/s |
Friction Coefficient |
0.05~0.15 |
||
Anti-tensile Strength |
150 N/mm² |
Heat-conducting Coefficient |
60 W/(m*k) |
||
Alloy hardness |
HB 45-70 |
Heat-expansion Coefficient |
19*10^-6k |
Content |
Cu |
Pb |
Sn |
Zn |
P |
Fe |
Ni |
Sb |
Others |
Remainder |
9-11 |
9-11 |
0.5 |
0.1 |
0.7 |
0.5 |
0.2 |
0.5 |