As the professional manufacturers, Top Bearings would like to provide you high quality Si3N4 Full Ceramic Bearings PTFE or PEEK Cage. And we will offer you the best after-sale service and timely delivery.
Si3N4 Full Ceramic Bearings PTFE or PEEK Cage
As the professional manufacturers, Top Bearings would like to provide you high quality Si3N4 Full Ceramic Bearings PTFE or PEEK Cage. And we will offer you the best after-sale service and timely delivery.
Si3N4 Full Ceramic Bearings PTFE or PEEK Cage have some better performance than ZrO2, the rings and balls made by full ceramic material: Si3N4, as a standard contracture, the cage made by PTFE, generally we also could make the cage with GFRPA66-25,PEEK,PI, Phonemic Textiles Tube ,etc. Compares than the material of ZrO2, Si3N4 Full Ceramic Bearings PTFE or PEEK Cage could endure heavier load and could be used in higher temperature environment. Also we could offer precision ceramic bearing which generally used in high-speed and high-rigidity spindle. The manufactured clearance could be P4 to UP grade.
Material: |
Si3N4 Ceramic Material |
Density: |
3.2 G/cm3 |
Material Of Rings & Balls: |
Full Si3N4 Ceramic Material |
Almost Material Of Cage: |
PTFE |
Other Material Of Cage: |
GFRPA66-25, PEEK, PI, Phonemic Textiles Tube ,etc. |
Application Temperature: |
1000℃ |
High Light: |
rod end bearing, plain bearing bush |
Technical data | unit | GCr15 | 9Cr18 | Si3N4 | AL203 | ZrO2 |
Density | g/cm³ | 7.8 | 7.9 | 3.2 | 3.95 | 6 |
a Coefficient of expansion | 10^-6/℃ | 11 | 17 | 3.2 | 9.1 | 10.5 |
E modulus of elasticity | Gpa | 208 | 200 | 320 | 380 | 210 |
μ Poisson ratio | 0.3 | 0.3 | 0.26 | 0.27 | 0.3 | |
HV Hardness | 800 | 700 | 1700 | 1800 | 1300 | |
δ Flexural strength | Mpa | 2400 | 2600 | 900 | 220 | 1000 |
δ Compressive Strength | MPa | 2000 | 1500 | 3500 | ||
Kc Impact strength | Nm/cm² | 20 | 25 | 7 | 3.5 | 11 |
λ Thermal conductivity | W/mk | 30-40 | 15 | 3.5 | 25 | 2.5 |
Ω Specific resistivity | mm²/m | 1 | 0.75 | 10^18 | 10^8 | 10^5 |
Specific heat | J/KgK | 450 | 450 | 800 | 880 | 400 |
Application temperature | ℃ | 120 | 150 | 1000 | 1850 | 800 |
Anti-corrossion | No | poor | Good | Good | Good | |
Cycle stress | 10*10^6 | 10*10^6 | 50*10^6 | 30*10^6 | 50*10^6 | |
Destroy model | peel | peel | peel | fracture | peel/fracture | |
Anti-magnetism | Yes | Yes | No | No | No | |
Dimension stability | bad | poor | Good | Good | Good | |
Insulate properties | No insulation | No insulation | Good | Good | Good |
Material | HDPE | PP | POM | PA66 | PVDF | PPS | PTFE | PEEK |
Long-time working temp. | 90 | 100 | 110 | 100 | 150 | 230 | 260 | 280 |
Density | g/cm3 | 0.91 | 1.42 | 1.14 | 1.77 | 1.35 | 2.18 | 1.32 |
Ball indentation hardness | 50 | 80 | 170 | 170 | 80 | 190 | 30 | |
Tensile stress | 25 | 30 | 70 | 80 | 50 | 75 | 25 | 95 |
Sliding friction coefficient | 0.29 | 0.3 | 0.34 | 0.35-0.42 | 0.3 | 0.08-0.1 | 0.3-0.38 | |
Melted temperature | 130 | 165 | 175 | 260 | 172 | 280 | 327 | 343 |
Short-time highest application temperature | 90 | 140 | 150 | 170 | 150 | 260 | 260 | 300 |
Coet of Inear expansion (10^-5/K) | 13-15 | 17 | 10 | 8 | 13 | 5 | 12 | 5 |
Dielectric constant at 1 Mhz(10^6HZ) | 2.4 | 2.25 | 3.7 | 3.6-5 | 8 | 2.1 | 3.2-3.3 | |
Volume resisrivity (Ω·cm) | >10^15 | >10^24 | >10^14 | 10^13 | 10^12 | >10^13 | 10^14 | 10^13 |
flammability UL94 | + | + | - | (+) | (+) | - | + | + |
Anti-weathering | - | - | - | - | - | - | + | - |
Note: + =resistant; (+) =partly resistant; - =non-resistant |